Abstract

Climelt Mo-30W is a 70% Mo-30% W alloy recommended for high temperature service, and resistance to molten zinc. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Mo-9. Producer or source: Climax Molybdenum Company of Michigan, American Metal Climax.