BETHLEHEM V STEEL comprises a family of high-strength, low-alloy, hot-rolled steels in various forms for construction and general purposes. These steels offer yield strengths ranging from 42,000 to 65,000 psi. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-257. Producer or source: Bethlehem Steel Corporation.