Abstract

CLIMELT MOLYBDENUM is a commercially pure high melting point metal for applications such as electronic tube components, electric furnace elements, electrical contacts, and electrodes. It is produced by arc casting. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Mo-10. Producer or source: Climax Molybdenum Company of Michigan, American Metal Climax.