MEEHANITE AQ is a wear and abrasion resisting iron that is readily machinable as cast but may be air hardened after machining with minimum distortion. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as fracture toughness and fatigue. It also includes information on high temperature performance as well as heat treating and machining. Filing Code: CI-36. Producer or source: Meehanite Metal Corporation.