Abstract

ALUMINUM 224.0 was developed for the production of sand and composite mold castings which will meet substantially higher elevated temperature strength requirements than other aluminum casting alloys. This datasheet provides information on composition, physical properties, tensile properties, and compressive and shear strength as well as fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-200. Producer or source: Aluminum Company of America.