Abstract

VAN LOM is a molybdenum type high-speed steel having excellent wear and cutting properties. It is recommended for cutting tools, punches, shear blades, blanking dies, etc. where improved toughness is desired. This datasheet provides information on composition, physical properties, hardness, and elasticity as well as fracture toughness, and deformation. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-222. Producer or source: Teledyne Vasco.