Abstract

Revere No. 464 is a copper-zinc alloy having good strength, toughness, and resistance to corrosion. It is recommended for steam condensers, marine equipment and oil refinery equipment, most especially in the form of sheet and plate, the latter as the heads for condensers and similar heat exchangers. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Cu-204. Producer or source: Revere Copper and Brass Inc..