Abstract
Elkaloy-A is a copper-base alloy having high strength and toughness coupled with high electrical and thermal conductivity. It is recommended for springs, electrical contacts and resistance welding electrodes. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: Cu-198. Producer or source: Mallory Metallurgical Company.
chemical composition, corrosion-resistant alloys, electrical conductivity, electrical contacts, Elkaloy-A, fatigue properties, fracture toughness, hardness, heat treatability, joinability, machinability, physical properties, springs, tensile properties, thermal conductivity, welding electrodes, workability