Abstract
BRUSII Alloy 200C is a beryllium-nickel casting alloy having high resistance to wear, corrosion, thermal shock and oxidation. It is recommended for fuel pump impellers, turbines, non-sparking tools, molds for plastics and glass. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Ni-142. Producer or source: Brush Beryllium Company.
BRUSH Alloy 200C, castability, chemical composition, corrosion-resistant alloys, elasticity, fracture toughness, fuel pump impellers, hardness, heat treatability, high-temperature alloys, joinability, machinability, molds, oxidation resistance, physical properties, tensile properties, thermal shock resistance, turbines, wear resistance
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
Topics
Molds
Corrosion-resistant alloys
High-temperature alloys
Cast nickel alloys
Nickel alloys
Chemical composition
Oxidation resistance
Castability
Heat treatability
Joinability
Machinability
Elastic modulus
Fracture toughness
Thermal shock resistance
Wear resistance
Hardness
Tensile properties
Physical properties
Thermal properties
Impellers
You do not currently have access to this content.