Columbium 15W-5 Mo- 1Zr is a columbium-base alloy capable of retaining usuable structural properties up to 2500 F. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Cb-17. Producer or source: Fansteel Metallurgical Corporation.