AISI C1060 is a high-carbon water or oil hardening tool and spring steel recommended for heavy machinery parts, shafts, springs and miscellaneous tools requiring strength and wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as heat treating, machining, and joining. Filing Code: CS-32. Producer or source: Carbon and alloy steel mills.