Abstract

ILZRO-14 is a zinc-base die casting alloy developed with superior creep resistance at both ambient and elevated temperatures. It is recommended for carburetors, fuel pumps, valve bodies, etc. This datasheet provides information on composition, physical properties, hardness, and tensile properties as well as creep. It also includes information on corrosion resistance as well as casting, machining, joining, and surface treatment. Filing Code: Zn-11. Producer or source: Zinc and zinc alloy suppliers.