Abstract

DELORO STELLITE-100 is a hard and abrasion resistant alloy designed specifically for metal cutting purposes. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength. It also includes information on corrosion resistance as well as casting, heat treating, and machining. Filing Code: Co-55. Producer or source: Deloro Stellite Ltd.