Abstract
HOWMET No. 3 is a cobalt-base alloy having high hardness and compressive strength, high heat and corrosion resistance, along with excellent abrasion and wear resistance. It is recommended for bushings, scrapers, valve parts, and other machinery components. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Co-56. Producer or source: Howmet Corporation Metal Products Division.
abrasion resistance, castability, chemical composition, compressive strength, corrosion-resistant alloys, elasticity, fracture toughness, hardness, heat resistance, heat treatability, Howmet no. 3, joinability, machinability, machinery components, physical properties, tensile properties, wear resistance
Copyright © ASM International® 1996
1996
ASM International
Topics
Mechanical and machine components
Corrosion-resistant alloys
Cobalt alloys
Chemical composition
Castability
Heat treatability
Joinability
Machinability
Compressive strength
Elastic modulus
Fracture toughness
Wear resistance
Abrasive wear resistance
Hardness
Tensile properties
Physical properties
Thermal resistance
You do not currently have access to this content.