Republic RSM-200 is a high strength, tough maraging steel recommended for airframe and missile systems. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SA-209. Producer or source: Republic Steel Corporation.