Abstract
PRESSURDIE-1 is an air-hardening hot work tool and die steel having high heat resistance and good high temperature strength properties. It is recommended for die casting dies, extrusion and forging dies. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: TS-191. Producer or source: Continental Copper & Steel Industries Inc..