Aluminum 8280 is a aluminum bearing alloy recommended for maximum operating temperature of 300 F. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on machining. Filing Code: Al-165. Producer or source: Aluminum Company of America.