Abstract

RMI-6A1-2Cb-1Ta-0.8Mo is a titanium-base alloy recommended for parts requiring high impact strength along with good corrosion resistance, especially for deep diving under sea vehicles. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: Ti-53. Producer or source: Reactive Metals Inc..