Cyclops L1 is an oil hardening chromium steel that is recommended for relatively short run tools and dies. It is tough and wear resistant. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-200. Producer or source: Cyclops Corporation.