Abstract

AISI 6130 is a chromium vanadium steel having good hardenability, fatigue resistance, and toughness. It is recommended for heavy duty equipment, gears, shafts, fasteners, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on casting, forming, heat treating, machining, and joining. Filing Code: SA-219. Producer or source: Alloy steel mills and foundries.