Abstract
DOFASCOLOY-P is a high-strength low-alloy steel characterized by excellent weldability, good atmospheric corrosion resistance and good resistance to brittle fracture. It is recommended for structures, bridges, earth moving equipment, etc. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive, shear, and bend strength as well as fatigue. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-218. Producer or source: Dominion Foundries & Steel Ltd.
bend strength, bridges, brittle fracture, chemical composition, compressive strength, corrosion, corrosion-resistant alloys, DOF Ascoloy-P, earth moving equipment, elasticity, fatigue properties, fracture resistance, hardness, heat treatability, joinability, machinability, physical properties, shear strength, tensile properties, weldability, workability
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
Topics
High-strength low-alloy steel
Buildings and bridges
Construction equipment
Corrosion-resistant alloys
Chemical composition
Heat treatability
Joinability
Machinability
Weldability
Workability
Bend strength
Compressive strength
Elastic modulus
Fatigue properties
Fracture toughness
Hardness
Shear strength
Physical properties
Thermal properties
You do not currently have access to this content.