NIMONIC 110 is a highly alloyed nickel-base alloy having high creep and oxidation resistance. It is recommended for aircraft gas turbine components to resist the stresses at the very high temperatures of operation. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-128. Producer or source: Henry Wiggin & Company Ltd.