Abstract

VERSASTEEL is a tool steel designed to provide an unusual combination of fine grain structure, high secondary hardness, and compressive yield strength together with good toughness and high wear resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-188. Producer or source: Crucible Steel Company of America.