Abstract

Tophet-D is an iron-nickel-chromium alloy recommended for electric furnace heating elements and electrical resistors operating up to 1600 F. This datasheet provides information on composition, physical properties, hardness, and tensile properties. It also includes information on high temperature performance as well as forming, heat treating, and machining. Filing Code: Fe-30. Producer or source: Wilbur B. Driver Company.