Crusible CCS is an air-hardening hot work steel having high temperature properties and heat resistance. It is recommended for die casting dies, forging and extrusion tools. This datasheet provides information on composition, physical properties, hardness, and elasticity. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: TS-182. Producer or source: Crucible Steel Company of America.