Uranus-50T is a chromium-nickel austenitic stainless steel having high resistance to acids and freedom from intergranular corrosion. It is recommended for the chemical, food and marine industries. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: SS-186. Producer or source: Usine de l'Ondaine.