Abstract

STELCOLOY-S is a high-strength low-alloy steel recommended where high yield strength combined with toughness are required in such applications as earth moving equipment, railroad and mine cars and bridges. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and bend strength. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: SA-198. Producer or source: The Steel Company of Canada Ltd.