Magnesium ZK21A is a non-hardenable extruded magnesium-base alloy having moderate strength and good weldability. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive strength. It also includes information on forming, heat treating, machining, and joining. Filing Code: Mg-60. Producer or source: The Dow Chemical Company, Metal Products Department.