TM-6 LOW CARBON is a modification of Type M-2 tungsten-molybdenum high-speed steel recommended for cold work or hot work applications. It is not intended for use as cutting tools. This datasheet provides information on composition and hardness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-175. Producer or source: H. K. Porter Company Inc..