Abstract
CUBE-ALLOY is a dispersion hardened copper recommended for high temperature electrical systems, such as motor windings, current carrying springs and welding electrode tips, where high electrical conductivity is required at elevated temperatures. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Cu-172. Producer or source: Handy & Harman.