Abstract
DELORO STELLITE-6 is a cobalt-base alloy having good resistance to wear and shock along with excellent corrosion resistance and high temperature strength. It is recommended for steam and chemical valves. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive strength as well as fracture toughness. It also includes information on high temperature performance and corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: Co-49. Producer or source: Deloro Stellite Ltd.
castability, chemical composition, compressive strength, corrosion-resistant alloys, Deloro Stellite-6, elasticity, fracture toughness, hardness, heat treatability, high-temperature alloys, joinability, machinability, physical properties, shock resistance, tensile properties, wear resistance, workability
This content is only available as a PDF.
Copyright © ASM International® 1996
1996
ASM International
Topics
Corrosion-resistant alloys
High-temperature alloys
Cobalt alloys
Chemical composition
Castability
Heat treatability
Joinability
Machinability
Workability
Compressive strength
Elastic modulus
Fatigue properties
Fracture toughness
Wear resistance
Hardness
Tensile properties
Physical properties
Thermal properties
You do not currently have access to this content.