Abstract

Ti-679 is a titanium high temperature alloy having an excellent combination of short-time strength, creep strength and stability to 900 F. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as creep. It also includes information on high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Ti-48. Producer or source: Titanium Metals Corporation of America.