Abstract

DURAMOLD-B is a low carbon, low alloy carburizing grade of steel recommended for hobbed plastic molds and dies. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, and joining. Filing Code: TS-169. Producer or source: Bethlehem Steel Corporation.