Magnesium-LA91 is a magnesium-lithium lightweight alloy recommended for missile and space vehicle structures. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, machining, and joining. Filing Code: Mg-58. Producer or source: Brooks & Perkins Inc..