Abstract

Nimocast 90 is a nickel-base casting alloy having useful creep resistance at temperatures up to 870 C. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, joining, and surface treatment. Filing Code: Ni-101. Producer or source: Henry Wiggin & Company Ltd.