Abstract
Nickelvac Super-X is a nickel-base alloy recommended for applications requiring oxidation and corrosion resistance coupled with good strength up to 1200-1500 F. It is used in gas turbines heat engines, high temperature bolts and forming tools. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as forming, heat treating, machining, joining, and surface treatment. Filing Code: Ni-98. Producer or source: Allvac Metals Company.