Abstract

Aluminum A132 is a high-silicon, nickel, aluminum-base alloy recommended for high strength permanent mold castings. It responds to an age-hardening heat treatment. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and shear strength as well as creep and fatigue. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Al-148. Producer or source: Aluminum Company of America.