Kennertium W-2 is a high density tungsten-base alloy having strength, rigidity, ductility and good machinability. It is recommended for gyro rotors, counterweights, governors, radiation shielding and similar applications. This datasheet provides information on composition, physical properties, elasticity, tensile properties, and compressive strength as well as creep. It also includes information on heat treating, machining, and joining. Filing Code: W-7. Producer or source: Kennametal Inc..