AUR-O-MET 56 is a nickel-aluminum bronze having high strength, wear and shock resistance, combined with good corrosion resistance. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness. It also includes information on corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: Cu-145. Producer or source: Aurora Metal Company.