Abstract

Alnico 8 is a permanent magnet material having over twice as much resistance to demagnetization as Alnico 5. It requires a magnetic heat treatment to develop strong directional magnetic properties. This datasheet provides information on composition, physical properties, and hardness. It also includes information on heat treating and machining. Filing Code: Co-39. Producer or source: Crucible Steel Company of America.