Abstract

Kentanium K138-A is a high temperature titanium carbide that greatly widens the scope of the engineering design where conditions of intermittent or continuous high temperatures in oxidizing atmospheres are combined with abrasion, and compressive or tensile loads. This datasheet provides information on composition, physical properties, hardness, elasticity, and compressive strength as well as fracture toughness, creep, and fatigue. It also includes information on machining and joining. Filing Code: Ti-40. Producer or source: Kennametal Inc..

This content is only available as a PDF.