Abstract

COMO is a high-speed steel designed to give much longer life in machining difficult to cut metals, such as superalloys and high heat resisting materials. This datasheet provides information on composition and hardness as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-148. Producer or source: Continental Copper & Steel Industries Inc..