Abstract
Cooper Alloy 14S is an abrasion, heat and corrosion resistant alloy steel containing 12% chromium. It can be hardened by heat treatment. It is recommended for pumps and valves in the cast form. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as fracture toughness and creep. It also includes information on high temperature performance and corrosion resistance as well as casting, heat treating, machining, and joining. Filing Code: SS-158. Producer or source: Cooper Alloy Corporation.