Abstract

Falcon-6 is a shock resistant tool and die steel having extreme toughness combined with wear resistance and fatigue resistance. It is recommended for cold battering tools and hot die applications. This datasheet provides information on composition, hardness, and tensile properties as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-147. Producer or source: Atlas Steels Company.