Abstract

UDIMET 41 is a vacuum induction melted precipitation hardening nickel-base alloy having outstanding room and elevated temperature properties. It possesses excellent corrosion and oxidation resistance. It is designed for highly stressed components operating in the 1400-1700 deg F temperature range. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties as well as creep. It also includes information on low and high temperature performance as well as forming, heat treating, machining, and joining. Filing Code: Ni-92. Producer or source: Special Metals Inc..