Abstract

Nivco 10 is a cobalt-base turbine alloy having a combination of high damping capacity, high strength and high ductility. It is a precipitation hardening alloy recommended for use at temperatures up to 1200 F, such as turbine blades. This datasheet provides information on composition, physical properties, elasticity, and tensile properties as well as fracture toughness, creep, and fatigue. It also includes information on forming, heat treating, machining, and joining. Filing Code: Co-37. Producer or source: Westinghouse Electric Corporation.