Bridgeport 54 is a copper-zinc-aluminum alloy having high corrosion and erosion resistance combined with good strength and ductility. This datasheet provides information on composition, physical properties, hardness, elasticity, and tensile properties. It also includes information on corrosion resistance as well as heat treating and machining. Filing Code: Cu-141. Producer or source: Bridgeport Brass Company.