Abstract

OREMET HPC 98W-2MO is a vacuum consumable electrode melted refractory tungsten alloy having 100% density. It is recommended where strength and/or corrosion resistance at high temperatures are required. This datasheet provides information on composition, physical properties, microstructure, hardness, elasticity, and tensile properties. It also includes information on high temperature performance and corrosion resistance as well as casting, forming, heat treating, machining, and joining. Filing Code: W-8. Producer or source: Oregon Metallurgical Corporation.