Abstract

GYROMET is a rungsten-bearing sintered alloy of high strength and density recommended for rotor applications. This datasheet provides information on composition, physical properties, hardness, elasticity, tensile properties, and compressive and bend strength as well as creep and fatigue. It also includes information on high temperature performance and corrosion resistance as well as heat treating, machining, and joining. Filing Code: W-6. Producer or source: Mallory Metallurgical Company.