Super Panther is a cobalt type high-speed steel recommended for heavy duty cutting of hard, gritty, cast irons and heat treated steels. This datasheet provides information on composition, physical properties, and hardness as well as fracture toughness. It also includes information on forming, heat treating, machining, and joining. Filing Code: TS-137. Producer or source: Allegheny Ludlum Corporation.